Precautions when using wire trimming function in EDM wire cutting machine tools Wire EDM cutting in EDM has increased the tool trimming function compared to EDM wire cutting. Used for cutting, the next few knives are used for finishing, so the use of EDM wire cutting machine can achieve a higher finish.
Because the electrode wire used in the wire-cutting machine tool in EDM is used repeatedly. When the knife repair function is used, as the cutting area increases, the electrode wire generates wire drawing and electrode wire loss, which will become thinner and thinner, which ultimately affects the accuracy of the work and the effect of the next few discharge cutting.
In order to obtain high accuracy, it is necessary to measure the actual diameter of the molybdenum wire before starting to cut. It is recommended to tighten the molybdenum wire after cutting the guide wire and before officially cutting the workpiece. If the molybdenum wire has been used repeatedly for a long period of time, the diameter and roundness of the molybdenum wire need to be measured. If the difference is too large, a new electrode wire must be replaced.
Pay attention to the following points when using multiple cuts:
1. When the molybdenum wire runs empty, check whether the molybdenum wire shakes.
2. Whether there are cutting marks on the surface of the conductive block, and whether the molybdenum wire is trapped in the conductive block.
3. Whether the working fluid flow and color are normal.
4. Before processing, the process needs to be simulated. Determine whether the cutting program generated by the system is true.
5. According to the characteristics of the material, the working cut-off amount of the last cut is as long as possible to reduce the influence of material deformation.
6. Several problems on the working surface after cutting:
① Line marks on the surface may be caused by jitter of the electrode wire or deformation of the material and unreasonable setting of the offset.
②The black spots on both ends of the working surface are serious, and the working fluid is a problem. It is recommended that you can try to use water-based cutting fluid.
③After cutting, please clean with oxalic acid in time, then rinse with water to remove oxalic acid residue. Wipe off the water stain with a clean white cloth, and finally apply anti-rust oil.

Hubungi kami

Author:

Mr. Kevin

Phone/WhatsApp:

+8618861016123

Produk populer
You may also like
Related Categories

Email ke pemasok ini

Subjek:
Ponsel:
Email:
Pesan:

Your message must be betwwen 20-8000 characters

Hak cipta © 2024 Suzhou Tiptop Machinery Technology Co. Ltd. semua hak dilindungi.

We will contact you immediately

Fill in more information so that we can get in touch with you faster

Privacy statement: Your privacy is very important to Us. Our company promises not to disclose your personal information to any external company with out your explicit permission.

Kirim